This additive is a pinkish liquid, used in the electrolytic coloring process after the anodization of Al profiles. By using this agent, it is easy to control the Rose Gold coloring processing with minimum color difference and better result in terms of abrasion-resistance, erosion-resistance and weather-resistance than that of the conventional champagne-colored ones. |
||
1. Bath Composition (For make-up): |
||
|
SN-4 |
10g/L |
2. Processing Parameters: |
||
|
SN-4 |
8-12g/L |
3. Bath Maintenance: |
||
|
(1) Analyze the contents of SN-4, free H2SO4 and make compensation in time. |